Dr. Angelique Lasseigne’s Publications

  1. D.L. Olson, G.R. Edwards, P. Bollinger, A.N. Lasseigne, and G. Atkins, “Materials and Practices to Improve Resistance to Fuel Derived Environmental Damage In Land and Sea- Based Turbines” Workshop Proceedings, EPRI Technical Report #1009173, pp.1-128, EPRI, Palo Alto, California,   October (2003).
  2. D.L. Olson, A.N. Lasseigne, M. Marya and B. Mishra, “ Weld Features that Differentiate Weld and Plate Corrosion”, Practical Failure Analysis Vol. 3 (5) October pp 43-57 (2003).
  3. Y.D. Park, A.N. Lasseigne, V.I. Kaydanov, D.L. Olson, A. Landau, M. Pinkas and B. Sarusi, “Thermoelectric Diagnostics for Nondestructive Evaluation of Materials”, Proceedings of 10th CF/DRDC Meeting on Naval Applications on Materials Technology, 13-15 May 2003, pp. 648-666, paper 46, DRDC Atlantic, (2003).
  4. D.L. Olson, A. N. Lasseigne, M. Marya, B. Mishra, “Fundamental Models for Corrosion in Fusion Welds- Emphasis on Interfacial and Gradient Effects”, in Joining of Advanced and Specialty Materials V, Conf. Proc. of Materials Solutions 02, 7-9 October 2002, Columbus, Ohio, pp. 1-11, ASM Intl, Materials Park, Ohio, 2003.
  5. D.L. Olson, A. N. Lasseigne, M. Marya, B. Mishra, and G. Castro, “Material Science Aspects of Weld Corrosion”, Proc. Intl. Conf. on Welding and Joining of Materials 2003, pp., Pontificia Universidad Catolica del Peru, Lima, Peru, October 27-29 (2003).
  6. D.L. Olson, A. N. Lasseigne, M. Marya, B. Mishra, and G. Castro, “Topicos en Ciencia de Materiales Corrosion de Soldaduras”, Proc. Intl Conf. on Welding and Joining of Materials 2003, pp. , Pontificia Universidad Catolica del Peru, Lima, Peru, October 27-29 (2003).
  7. A.N. Lasseigne, “Non-Destructive Determination of Interstitial Nitrogen Content in Austenitic Stainless Steel Weld Metal Utilizing Thermoelectric Power”, Masters Thesis, T-, May 2004.
  8. A.N. Lasseigne, D.L. Olson, T. Boellinghaus, Hans-Joachim Kleebe and R. D. Smith, “Non-Destructive Determination of Nitrogen in Nitrogen Strengthened Austenitic Stainless Steel Weldments Utilizing Thermoelectric Power coefficient Measurements”, in Proc. Intl. Conf. High Nitrogen Steels 2004, pp. 577-583, Ostend, Belgium (2004), GRIPS Media GmbH, Bad Harzburg, Germany (2004).
  9. A.N. Lasseigne, D.L. Olson, Th. Boellinghaus, and V. I. Kaydanov, “Utilization of Non-destructive Thermoelectric Power Measurements for Determination of Interstitial Nitrogen Content in Nitrogen-Strengthened Austenitic Stainless Steel Welds”, in Proc. QNDE Conf. 2004, CSM, Golden, Colorado, American Institute of Physics, Melville, N. Y. (2004).
  10. D. Park, D. L. Olson, B. Mishra and A. N. Lasseigne, Thermoelectric Power Assessment of Weld Microstructure, Phase Stability, Residual Stress and Properties”, in Proc. Intl. Conf. on Trends of Welding Research, MAY 16-20, 2005, Pine Mtn., Georgia, pp. 497-505, ASM, Materials Park, OH, (2006).
  11. N. Lasseigne, D. L. Olson and Th. Boellinghaus, “Techniques for Determination of Interstitial Nitrogen Content in Nitrogen Strengthened Austenitic Stainless Steel Alloy 1.4565”, in Proc. of Intl. Conf. on Trends in Welding Research, May 16-20,2005, Pine Mtn., Georgia, pp. 799-806, ASM, Materials Park, OH, (2006).
  12. A.N. Lasseigne, D.L. Olson, and Th. Boellinghaus, “ Development of a Non-Destructive Tool for Assessment of Residual Stress in Welds”,Proc. of ASNT Fall Conf. 2004 , pp 141-143, Las Vegas, NV, USA, 15-19, November (2004), ASNT, Columbus, OH, (2004).
  13. Smith, T. Siewert, B. Mishra, D. Olson, and A. Lasseigne, ‘Coatings for Offshore Protection: Offshore Oil and Gas Operation Facilities, Marine Pipeline, and Ship Structures, April 14-16, 2004, Biloxi, MS, NIST Special Publication 1035 (2005).
  14. Lasseigne, A.N., Olson, D.L., Kleebe, H.J., and Boellinghaus, Th., “Microstructural Assessment of Nitrogen-Strengthened Austenitic Stainless Steel Welds Utilizing Thermoelectric Power”, Metallurgical and Material Transactions A, Metallurgical and Materials Transactions A, Vol. 36A, November, pp. 3031-3039, (2005).
  15. Moline, J. Scott, A.N. Lasseigne, S. Liu, “Effect of Copper Additions in HSLA Steel Welds”, AWS 2005,
    November 14-17, Chicago, Illinois.
  16. J.E. Jackson, A.N. Lasseigne, D.L. Olson, S. Liu, “Engineering Weld Design – Are Hybrid Welding Wires in our Future?”, AWS 2005, November 14-17, Chicago, Illinois.
  17. A.N. Lasseigne, I. Ashraf, B. Mishra, and D.L. Olson Characterization of Hydrogen Storage Capabilities of the Two-Phase Region of LaNi5“, paper and presentation accepted for TMS 2006: Linking Science and Technology for Global Solutions in San Antonio, Texas.
  18. A.N. Lasseigne, I. Ashraf, B. Mishra, D.L. Olson, V. Kaydanov, and R. Goldfarb, “Characterization of Hydrogenation Behavior of NaAlH4 Utilizing Thermoelectric Power and Magnetic Analyses” paper and presentation accepted for TMS 2006: Linking Science and Technology for Global Solutions in San Antonio, Texas.
  19. J.E. Jackson, A.N. Lasseigne, D.L. Olson, B. Mishra, and V.Kaydanov, “Characterization of Engineering Materials   Utilizing Thermoelectric Power Measurement”, paper and presentation accepted for TMS 2006: Linking Science and Technology for Global Solutions in San Antonio, Texas.
  20. A.N. Lasseigne, K. Moline, J. Scott, J. Rawers, J.E. Jackson, D.L. Olson, and B. Mishra, Synergistic Interstitial Control of Sensitization and Pitting in Stainless Steel Weldments, Stainless Steel World, Houston, Texas, November 2006.
  21. A.N. Lasseigne-Jackson, D.L. Olson, B. Mishra, J.E. Jackson Development of Electromagnetic Techniques for Hydrogen Content Assessment in Coated Linepipe Steel, QNDE 2006, Houston, Texas, American Institute of Physics, To be Published.
  22. Mishra, A. N. Lasseigne, and D. L. Olson, “Role of Solidification on Nitrogen-Strengthened Austenitic Stainless Steel Weldments”, Proc. International Conference on Solidification Science and Processing Emerging Trends 9, ICSSP III), Nov. 19-23, 2006, Jaipur, India. (2006).
  23. L. Olson, Y. D. Park, J. E. Jackson, and A. N. Lasseigne-Jackson, “ Engineered Weld Design: Are Composite Welds Likely in the Future”, Proceedings Korean Intl. Welding Conf. 2007. Seoul, Korea, (2007).
  24. D. Park, A. N. Lasseigne-Jackson, J. E. Jackson, B. Mishra, D. L. Olson, and T. Koenig, “Characterization of Weldments Using Thermoelectric Power Measurements”, Proceeding of Korean Intl. welding Conf. 2007, Soeul, Korea (2007).
  25. J.E. Jackson, A. N. Lasseigne, B. Mishra, and D.L. Olson, “The Influence of High Magnetic and Electric Fields on Hydrogen Content from Aqueous Corrosion Processes in Steel: Possible Mechanistic Interpretations”, Colorado School of Mines Research Report CSM-ACSEL-006-003, Prepared for MMS-OPS-NIST Pipeline Research Meeting at CSM, Jan. 24, 2006 (2006).
  26. J.E. Jackson, A.N. Lasseigne-Jackson, F.J. Sanchez, D.L. Olson, and B. Mishra, “Inspection-Related Magnetization Effect on Corrosion in Linepipe Steel: Thermodynamic and Kinetic Interpretations”, Proceedings of the American Society for Non-Destructive Testing Fall 2006 Conference, October 23-27 (2006).
  27. J.E. Jackson, D.L. Olson, A.N. Lasseigne-Jackson, B. Mishra , and T.A. Siewert, “Correlating the Influence of Magnetic Field on Solute Content in Metals Using the Thermodynamic Auxiliary Work Functions”, Properties and Processes for a Hydrogen-based Economy, Sixteenth Symposium on Thermophysical Properties, July 30 – August 4, 2006, Boulder, Colorado, U.S.A.
  28. J.E. Jackson, A.N. Lasseigne-Jackson, F.J. Sanchez, D.L. Olson, and B. Mishra, “The Influence of Magnetization on Corrosion in Pipeline Steels”, Proceedings of the 6th International Pipeline Conference, September 25-29, 2006, Calgary, Alberta, Canada (2006).
  29. A.N. Lasseigne-Jackson, J. Anton, J.E. Jackson, D.L. Olson, and B. Mishra, “Development of Electromagnetic Techniques for Hydrogen Content Assessment in Coated Linepipe”, Rev. QNDE 2006, pp. 1159-1164, American Institute of Physics, Melville, N. Y. (2007).
  30. J.E. Jackson, D.L. Olson, A.N. Lasseigne-Jackson, B. Mishra, and T.A. Siewert, “Using the Thermodynamic Auxiliary Work Functions to Correlate the Magnetic Field Influence on Solute Content in Metals”, to be published in the International Journal of Thermophysics (2007).
  31. J.E. Jackson, D.L. Olson, B. Mishra, and A.N. Lasseigne, “Deposition of Al-Si Metallic Coating Precursors on Mo-Si-B Turbine Materials”, TMS 2006 Annual Meeting, MPMD 7th Global Innovations Proceedings: Trends in Materials R&D for Sensor Manufacturing Technologies, Edited by I.E. Anderson, N.R. Moody, J.W. Sears, D.F. Bahr, H.L. Fraser, and J.E. Smugeresky, TMS (The Minerals, Metals & Materials Society) Annual Meeting, pp. 39-48 (2006).
  32. J.E. Jackson, Y.D. Park, A.N. Lasseigne, C. Sangphagdee, D.L. Olson, B. Mishra, and V. Kaydanov, “Characterization of Engineering Materials Utilizing Thermoelectric Power Measurements”, Materials in Clean Power Systems: Applications, Corrosion, and Protection, Edited by Z.G. Yang, K.S. Weil, and M.P. Brady, TMS (The Minerals, Metals & Materials Society) Annual Meeting, pp. 1-10 (2006).
  33. J.E. Jackson, D.L. Olson, B. Mishra, and A.N. Lasseigne-Jackson, “Deposition and Characterization of Al-Si Metallic TBC Precursor on Mo-Si-B Turbine Materials”, accepted for publication in International Journal of Hydrogen Energy, November (2006).
  34. A.N. Lasseigne, B. Mishra, D.L. Olson, and A. Zamarron, “Development of Sensors for Reversible Battery Hydrogen Storage Materials” International Congress on Innovative Solutions for the Advancement of the Transport Industry, San Sebastian, Spain, September (2006).
  35. J.E. Jackson, D.L. Olson, B. Mishra, and A.N. Lasseigne-Jackson, “Development of Advanced Thermal Barrier Coatings for Mo-Si-B materials”, in the proceedings of TMS 2007 Conference, Orlando, FL, February 27-March 1, 2007.
  36. J.E. Jackson, A.N. Lasseigne-Jackson, T. Koenig, D.L. Olson, and B. Mishra, “Development of Graded-Architecture Mullite Thermal Barrier Coating on Mo-Si-B Turbine Materials”, presented at ASME Turbo Expo 2007 November (2007).
  37. D.L. Olson, A.N. Lasseigne-Jackson, J.E. Jackson, B. Mishra, T. Koenig, and J.C. Madeni, “Weld Assessment by Thermoelectric Power Measurements”, for publication in the proceedings of the International Conference of Welding and Joining of Materials 2007, Cusco, Perú 16 – 18 April 2007.
  38. D.L. Olson, A.N. Lasseigne-Jackson, J.E. Jackson, T. Koenig, E. Soderstrom, and J.C. Madeni, “Engineered Weld Design: Use of Composite Concepts”, in the proceedings of the International Conference of Welding and Joining of Materials 2007, Cusco, Perú 16 – 18 April 2007.
  39. D.L. Olson, Y.D. Park, J.E. Jackson, and A.N. Lasseigne-Jackson, “Engineered Weld Design: Are Composite Welds Likely in the Future?” in the proceedings of the International Joining and Welding Conference, Korea, May 10-12, 2007.
  40. A.N. Lasseigne-Jackson, B. Mishra, D.L. Olson, and J.E. Jackson, “Reversible Hydrogen Storage Battery Materials: Non-Destructive Sensor Development”, Proceedings of the National Hydrogen Association, San Antonio, TX, March 19-22, 2007.
  41. A.N. Lasseigne-Jackson, B. Mishra, and D.L. Olson, “Characterization of Hydrogen Storage Capabilities in Advanced Battery Materials”, Materials and Manufacturing Processes, 22, pp, 433-439, 2007.
  42. A.N. Lasseigne, A. Zamarron, I. Ashraf, B. Mishra, D.L. Olson, “Development of Advanced Thermoelectric
    Power Hydrogen Sensors for Reversible Hydrogen Storage Materials”, PRICM-6, Sixth International Pacific Rim, Nov. 5-9, 2007, ICC Jeju, Jeju Island, Korea.
  43. A.N. Lasseigne and D.L. Olson, “Determination of Interstitial Nitrogen Content in Austenitic Stainless Steel Welds by Thermoelectric Power”, Brazilian Journal Soldagem and Inspecao, (2007).
  44. A.N. Lasseigne-Jackson, B. Mishra, and D.L. Olson, “Characterization of Hydrogen Storage Capabilities in Advanced Battery Materials”, Materials and Manufacturing Processes, 22, pp, 433-439, (2007).
  45. J.E. Jackson, B. Mishra, D.L. Olson, A.N. Lasseigne, and T. Siewert, “The Future of Microstructural Characterization: An Electronic Metallography Laboratory”, QNDE 2007, Golden, Colorado, AIP, (July, 2007), In press.
  46. A.N. Lasseigne, J.M. Anton, T.A. Siewert, D.L. Olson, B. Mishra, and J.E. Jackson, “Advanced Non-Destructive Measurement Scheme to Actively Monitor Hydrogen Content in Steel Pipelines”, QNDE 2007, Golden, Colorado, AIP, (July, 2007), In press.
  47. Landau, M. Pinkas, A.N. Lasseigne, D. Olson, “Developing a Monitoring Tool to Assess the Fatigue Damage in Ni-Based Superalloys Using Thermoelectric Electric Power Measurements”, QNDE 2007, Golden, Colorado, AIP, (July, 2007), In press.
  48. D.L. Olson, V. Kaydanov, A.N. Lasseigne, A. Landau, and M. Pinkas, “Application of Interdisciplinary Fundamentals to Achieve New Insight into Materials Properties, Stability, and Integrity”, QNDE 2007, Golden, Colorado, AIP, (July, 2007), In press.
  49. A.N. Lasseigne-Jackson, K. Moline, J. Scott, J. Rawers, J. E. Jackson, D. L. Olson, and B. Misha, “Synergistic Interstitial Control of Sensitization and Pitting in Stainless Steel Weldments”, Proc. Of Stainless Steel World 2006, pp. 1-8, Houston, TX, November 14 (2006).
  50. Mishra, A.N.Lasseigne and D. L. Olson, “Role of Solidification on Nitrogen-Strengthened Austenitic   Stainless Steel Weldments”, Proc. International Conference on Solidification Science and Processing- Emerging Trends 9ICSSP III), Nov. 19-23, 2006, Jaipur, India. (2006).
  51. J.E. Jackson, D.L. Olson, B. Mishra, and A.N. Lasseigne-Jackson, “Development of Advanced Thermal Barrier Coatings for Mo-Si-B materials”, TMS 2007 Proceedings, Orlando, FL, February 27-March 1, 2007.
  52. D.L. Olson, A.N. Lasseigne-Jackson, J.E. Jackson, B. Mishra, T. Koenig, and J.C. Madeni, “Weld Assessment by Thermoelectric Power Measurements”, Proceedings of the International Conference of Welding and Joining of Materials 2007, Cusco, Perú 16 – 18 April 2007.
  53. D.L. Olson, A.N. Lasseigne-Jackson, J.E. Jackson, T. Koenig, E. Soderstrom, and J.C. Madeni, “Engineered Weld Design: Use of Composite Concepts”, Proceedings of the International Conference of Welding and Joining of Materials 2007, Cusco, Perú 16 – 18 April 2007.
  54. Y.D. Park, A.N. Lasseigne-Jackson, J.E. Jackson, B. Mishra, D.L. Olson, and T. Koenig, “Characterization of Weldments and Materials Using Thermoelectric Power Measurements” in the Proceedings of the International Joining and Welding Conference, Korea, May 10-12, 2007.
  55. D.L. Olson, Y.D. Park, J.E. Jackson, and A.N. Lasseigne-Jackson, “Engineered Weld Design: Are Composite Welds Likely in the Future?” for publication in the proceedings of the International Joining and Welding Conference, Korea, May 10-12, 2007.
  56. E. Jackson, D. L. Olson, S. Liu, R. L. Hellner, A. N. Lasseigne-Jackson, and G. C. Trickel,“ Calibration of Electronic Property Measurements with Larson-Miller Parameter for Service Life Assessment”, Proc. of Boiler Tube and HRSG Tube Failure and Inspection Conference, Calgary, Alberta, Canada, EPRI, Palo Alto, California, October (2007).
  57. A.N. Lasseigne, J.E. Jackson, D.L. Olson, and B. Mishra, “Non-Destructive Hydrogen Storage Material Fuel Gauge and Diagnostic Tools”, SAE, October 30-Nov. 1, 2007, Rosemount, Illinois
  58. J.E. Jackson, A.N. Lasseigne-Jackson, T. Koenig, D.L. Olson, and B. Mishra, “Development of Graded-Architecture Mullite Thermal Barrier Coating on Mo-Si-B Turbine Materials”, Presented at ASME Turbo Expo 2007 November (2007).
  59. A.N. Lasseigne, A. Zamarron, I.Ashraf, B. Mishra, and D.L. Olson, “Thermoelectric Power Hydrogen Sensors for Reversible Hydrogen Storage Materials”, PRICM-6, Sixth Pacific Rim International Conference on Advanced Materials and Processing, ICC Jeju, Jeju Island, Korea, Nov. 5-9, 2007.
  60. D.L. Olson, Y.D. Park, S. Liu, J.E. Jackson, A.N. Lasseigne-Jackson, and E.A. Metzbower, “Engineered Weld Design: Are Composite Welds Likely in the Future?”, proceedings of the International Joining and Welding Conference, Korea, May 10-12, 2007.
  61. D.L. Olson, Y.D. Park, S. Liu, J.E. Jackson, and A.N. Lasseigne-Jackson, E. Metzbower, “Engineered Weld Design: Are Composite Welds Likely in the Future?”, Materials Science Forum, Vols. 580-582, pp. 307-310 (2008).
  62. A.N. Lasseigne, K. Koenig, D. McColskey, T. Siewert, D.L. Olson, J.E. Jackson, and B. Mishra, “Advanced Non-Destructive Hydrogen Content Sensors”, ACerS, Materials Innovations in an Emerging Hydrogen Economy, Cocoa Beach, 2008.
  63. D.L Olson, B. Mishra, S. Liu, A.N. Lasseigne-Jackson, J.E. Jackson, K. M.-S. Koenig, J.A. Roubidoux and R.H Hellner, “Advanced Quantitative Non-Destructive Assessment of Heat Treated 91 and 92 Steel Boiler Tubes, in Proc of Grade 91/92 Steel Workshop on grade 91/92 Boiler Steel,” Clearwater, Florida, April 7-9 2008, Electric Power Research Institute, EPRI, Charlotte, N.C. (2008)
  64. A.N. Lasseigne, J.D. McColskey, National Institute of Standards and Technology, Boulder, CO; K. Koenig, J. Jackson, D. Olson, B. Mishra, Colorado School of Mines, Golden, CO, “Advanced Non-Contact Diffusible Hydrogen Sensors for Steel Weldments” ASM Trends in Welding Research, Pine Mountain, Georgia, 2008.
  65. L. Olson, J. E. Jackson, B. Mishra, M. J. Kaufman, Colorado School of Mines, Golden, CO; T. A. Siewert, A. N. Lasseigne-Jackson, National Institute of Standards and Technology, Boulder, CO; M. Pinkas, A. Landau, Nuclear Research Center, Beer Sheva, Israel “Generation II Materials Science for Welds and Advanced Materials” ASM Pine Mountain, Trends in Welding Research, Pine Mountain, Georgia, 2008.
  66. N. Lasseigne, K. Koenig, D. L. Olson, J. E. Jackson, and B. Mishra, “Real-Time Low Frequency Impedance Measurements for Determination of Hydrogen Content in Pipeline Steel”, Quantitative Non-Destructive Evaluation 2008, Chicago, Illinois, AIP.
  67. E. Jackson, J. A. Roubidoux, B. Mishra, D. L. Olson, and A. N. Lasseigne, “Assessment of Magnetocorrosion by Magnetic and Impedance Measurements” Quantitative Non-Destructive Evaluation 2008, Chicago, Illinois, AIP.
  68. J.E. Jackson, D.L. Olson, B. Mishra, A. J. Roubidoux and A.N. Lasseigne, “Magnetocorrosion of Pipeline Steel”, Proc. I H.C. Hydrogen 2008, pp 1-9.
  69. A.N. Lasseigne, K. Koenig, D. McColskey, J. Jackson, D. Olson, B. Mishra, T. Siewert, “Non-Destructive Determination of the Diffusion Coefficient of Hydrogen”, Proceedings of the 2008 International Hydrogen Conference: Effects of Hydrogen on Materials, Eds. B. Somerday, P. Sofronis, and R. Jones, pp. 524-531.
  70. Jackson, J. Roubidoux, D. Olson, B. Mishra, A. Lasseigne-Jackson, “Magnetocorrosion of Pipeline Steel”, 2008 International Hydrogen Conference: Effects of Hydrogen on Materials, Proceedings of the 2008 International Hydrogen Conference: Effects of Hydrogen on Materials, Eds. B. Somerday, P. Sofronis, and R. Jones, pp. 540-547.
  71. Ph., Darcis, J.D., McColskey, A.N., Lasseigne, and T.A., Siewert, “Hydrogen Effects on Fatigue Crack Growth Rate in High Strength Pipeline Steel”, 2008 International Hydrogen Conference: Effects of Hydrogen on Materials, Proceedings of the 2008 International Hydrogen Conference: Effects of Hydrogen on Materials, Eds. B. Somerday, P. Sofronis, and R. Jones, pp. 381-388.
  72. A.N. Lasseigne and D.L. Olson, “Development of Nondestructive Techniques for Characterization of Residual Stresses in Advanced Materials”, Materials Evaluation, October, (2008), pp 1077-1083.
  73. T.A. Siewert, J. McColskey, A.N. Lasseigne, “Hydrogen Pipeline Research at NIST”, National Hydrogen Association Meeting, March 30-April 3, 2008, Sacramento, California.
  74. T.A. Siewert, A.N. Lasseigne, A.J. Slifka, J.D. McColskey, N.E. Nanninga, and Y. Levy, “Hydrogen-Steel Compatibility Research at NIST-Boulder”, March 30-April 3, 2009, Columbia, South Carolina.
  75. Koenig, A.N. Lasseigne, J.W. Cisler, B. Mishra, and D.L. Olson, “Non-Contact Non-Destructive Hydrogen and Microstructural Assessment of Steel Welds,” Proc. EPRI Welding Conference, Ft. Myers, FL (2009).
  76. Koenig, A.N. Lasseigne, Joseph Cisler, D.L. Olson and B. Mishra, “In-Situ Hydrogen Analysis in Weldment: Novel NDE for Weld Inspection”, DOT PHMSA, “OPS Accomplishments” http://primis.phmsa.dot.gov/rd/duccess.html. (March 2009).
  77. J.E. Jackson, D.L. Olson, B. Mishra, J. A. Roubidoux, and A.N. Lasseigne, “The Effects of High Magnetic and Electric Fields on Ingress and Magnetocorrosion in Pipeline Steel” Research Letters in Materials Science, 5 pages, (2009).
  78. A.N. Lasseigne and J.E. Jackson, “Use of Non-Destructive Hydrogen Content Sensors to Monitor Material Integrity”, NACE, Proceedings of Corrosion 2010, March 14-18, San Antonio, TX (2010)
  79. Koenig, Angelique N. Lasseigne, Joseph W. Cisler, Brajendra Mishra, Robert H. King, David L. Olson, “Non-contact, nondestructive hydrogen and microstructural assessment of steel welds”, International Journal of Pressure Vessels and Piping, Volume 87, Issue 11, November 2010, Pages 605-610.
  80. Kiattisaksri, P. J. Gibbs, K. Koenig, E. A. Pfeif, A. N. Lasseigne, P. F. Mendez, B. Mishraand D. L. Olson, ASSESSMENT OF THE STATE OF PRECIPITATION IN ALUMINUM CASTING A356.2 ALLOY USING NONDESTRUCTIVE MICROSTRUCTURE ELECTRONIC PROPERTY MEASUREMENTS, AIP Conf. Proc. 1211 , 1285 (2010)
  81. A. Roubidoux, J. E. Jackson, A. N. Lasseigne, B. Mishraand D. L. Olson, “NONLINEAR ANALYTICAL MODELING OF INTERFACIAL PHENOMENON AND NANO‐SIZE MICROSTRUCTURAL FEATURES TO BETTER CORRELATE NDE ELECTRONIC PROPERTY MEASUREMENTS TO MATERIAL STATE, AIP Conf. Proc. 1211 , 1277 (2010)
  82. Koenig, J. W. Cisler, A. N. Lasseigne, R. H. King, B. Mishraand D. L. Olson, NONDESTRUCTIVE, NON‐CONTACT HYDROGEN CONTENT ASSESSMENT OF COATED STEEL LINEPIPE WELDS, AIP Conf. Proc. 1211, 1167 (2010).
  83. M. Koenig, A.N. Lasseigne, D.L. Olson, J.E. Jackson, J.D. McColskey, R.H. King, and B. Mishra, “Non-destructive Hydrogen Sensors to Prevent Material Degradation from Hydrogen Damage”, in Proceedings of the 8th International Pipeline Conference, IPC2010-31283 (2010).
  84. A.N. Lasseigne, K.M. Koenig, J.E. Jackson, J. Scott, and K. Moline, “Advanced Quantitative Hydrogen Sensors for Characterization of Wrought Metal and Weldments for Offshore Structures”, Proceedings of Offshore Technology Conference, OTC-21974-PP (2010).
  85. A.N. Lasseigne and J.E. Jackson, “Use of Non-Destructive Hydrogen Content Sensors to Monitor Material Integrity”, 2010 NACE Conference Papers (NACE International), March 01, 2010, Pages: 1 – 15.
  86. E.A. Pfeif, A.N. Lasseigne, K. Krzywosz, E.V. Mader, B. Mishra, D.L. Olson,   “Characterization of Hydrogen Content in ZIrcaloy 4 Nuclear Fuel Cladding,” ,” AIP Conference Proceedings Vol 1211, Review of Progress in Quantitative Nondestructive Evaluation Conference Proceedings, Rhode Island, Vol. 29, (2010), pp. 1317-1324.
  87. E.A. Pfeif, Z. Jones, A.N. Lasseigne, K.Koenig, K. Krzywosz, E.V. Mader, S. Yagnik, B. Mishra, and D.L. Olson, “Submerged Eddy Current Method of Hydrogen Content Evaluation of Zircaloy-4 Fuel Cladding,” AIP Conference Proceedings, Vol. 1355, Review of Progress in Quantitative Nondestructive Evaluation, Vol. 30A, (2011) pp.168-175.
  88. A.N. Lasseigne, K.M. Koenig, J.E. Jackson, and J.D. McColskey, “In-Situ Electromagnetic Hydrogen Sensors to Prevent Stress Corrosion Cracking in Metals”, NACE, Proceedings of Corrosion 2011, March 13-17, San Antonio, TX (2011)
  89. Koenig, A. N. Lasseigne, J. E. Jackson, D. L. Olsonand B. Mishra, ”A FUNDAMENTAL ANALYSIS OF LOW FREQUENCY IMPEDANCE PHENOMENON: APPLICATION TO HYDROGEN CONTENT ASSESSMENT OF COATED LINEPIPE STEEL WELDMENTS”, AIP Conf. Proc. 1335 , 1163 (2011)
  90. A.N. Lasseigne, J.E. Jackson, K.M. Koenig, and J. Morrell, “Advanced Electromagnetic Sensors to Monitor Changes in Material Properties”, to be published in proceedings of IEEE Nuclear Science Symposium, 2011.
  91.  J.S. Morrell, A.N. Lasseigne, K. M. Koenig, and J.E. Jackson, “Noncontact Sensors for Detection of Radioactive Materials”, to be published in proceedings of IEEE Nuclear Science Symposium, 2011.
  92.  Meir, S. Liu, B. Mishra, D.L. Olson, A.N. Lasseigne, K. Coleman, R. Hellner, Advances in Materials Technology for Fossil Power Plants: Proceedings from the Sixth International Conference 2010 (ASM International), March 01, 2011, Pages: 554 – 570.
  93. Queen, H., J. K. Van Velsor, E. Giannini, and Concrete Durability Center. “NOVEL ELECTROMAGNETIC SENSORS FOR STRESS MEASUREMENT AND MATERIALS TESTING.” 9th International Conference on NDE in Relation to Structural Integrity for Nuclear and Pressurized Components, May 22-24, 2012 – Seattle, Washington, USA
  94.  Lasseigne, A.N., E.R. Giannini, and J. Jackson., Non-Contact Strain Measurements of Steel Reinforcement in Concrete Structures, ACI Special Publication: Advanced Materials and Sensors towards Smart Concrete Bridges: Concept, Performance, Evaluation, and Repair, 2013, (in press).
  95. RESEARCH REPORTS
  96. L. Olson, B. Mishra, and A. N. Lasseigne, “Development of a Non-Destructive, Non-Contact Electromagnetic Sensor for Hydrogen Content Determination in Coated Line Pipe Steel”, Progress Report for MMS Contract Number: 1435-01-04-36637, submitted to MMS. Herndon, VA and DOT-OPS, Washington DC, December 28, 2005.
  97. E. Jackson, A. N. Lasseigne, B. Mishra, and D. L. Olson, “The Influence of High Magnetic and Electric Fields on Hydrogen Content from Aqueous Corrosion Processes in Steel: Possible Mechanistic Interpretations”, Research Report # CSM-ACSEL-006-003, Prepared for MMS-OPS NIST Meeting at CSM, January 24, 2006.
  98. J.E. Jackson, A. N. Lasseigne, B. Mishra, and D.L. Olson, “The Influence of High Magnetic and Electric Fields on Hydrogen Content from Aqueous Corrosion Processes in Steel: Possible Mechanistic Interpretations”, Colorado School of Mines Research Report CSM-ACSEL-006-003, Prepared for MMS- OPS-NIST Pipeline Research Meeting at CSM, January. 24, (2006).
  99. S. Tordonato, D. L. Olson, and B. Mishra, “ABS Database of Corrosion Wasteage for Double Hull Tankers”, Technical Report, CSM Report # MT-CWJCR-006-004, submitted to ABS, Houston, TX, July (2006).
  100. L. Olson, B. Mishra, K. M. Evans, D. E. Dooley, A. N. Lasseigne-Jackson, J.E .Jackson, C. Sangphagdee, Y. D. Park, and C. A. VanHorn, “Thermoelectric Power Nondestructive Analysis for Nuclear Materials Applications “, NNSA POSTER, Washington D. C. October 11, 2006.
  101. E. Jackson, A. N. Lasseigne-Jackson, B. Mishra, D. L. Olson, C. M. Jensen, M. Kuba and S. A. Imam, “Fuel Sensors for Reversible Battery Hydrogen Storage Materials”, TMS 2007, Poster. Orlando, FL. (February 27, 2007).
  102. D.L. Olson, B. Mishra, A.N. Lasseigne-Jackson, M.S. Heilig, C. Ellis, C. Nguyen, R. Jones, and G. Garner, “Development of Advanced Austenitic Stainless Steels for Down-hole Applications”, CSM Report # MT-CWJCR-007-002 (2007).
  103. L. Olson, B. Mishra, K. M. Evans, D. E. Dooley, A. N. Lasseigne-Jackson, J.E. Jackson, C. Sangphagdee, Y. D. Park, and C. A. VanHorn, “Thermoelectric Power Non Destructive Analysis for Material Applications”, TMS 2007, Poster, Orlando, February 27 (2007) Orlando, FL. (Feb. 2007).
  104. J.E. Jackson, A. N. Lasseigne, B. Mishra, and D.L. Olson, “The Influence of High Magnetic and Electric Fields on Hydrogen Content from Aqueous Corrosion Processes in Steel: Possible Mechanistic Interpretations”, Colorado School of Mines Research Report CSM-ACSEL-006-003, Prepared for MMS-OPS-NIST Pipeline Research Meeting at CSM, Jan. 24, 2006 (2006).
  105. J.E. Jackson, A.N. Lasseigne-Jackson, B. Mishra, D.L. Olson, C.M. Jensen, M. Kuba, and S.A. Imam, “Fuel Sensors for Reversible Battery Hydrogen Storage Materials”, Poster: Materials Processing and Manufacture Division at TMS 2007 Conference, February 27, 2007, Orlando, FL.
  106. L. Olson, B. Mishra, A.N. Lasseigne-Jackson, M.S. Heilig, C. Ellis, C. Nguyen, R. Jones, and G. Garner, “Development of Advanced Austenitic Stainless Steels for Down-hole Applications”, CSM Report # MT-CWJCR-007-002 (2007).
  107. A.N. Lasseigne and J.E. Jackson, Hydride Formation in Alpha Titanium and Titanium Alloys, Materials Technology Institute, (2011), ISBN: 978-57698-055-2

Related Images: